Phone
+82-2-858-9890
Email
cs@dbmaterial.com
Fax
+82-2-6280-1988

News

CD-110 launched: a flexible non-combustible sheet to replace mica

In May 2026 we launched CD-110, a flexible non-combustible sheet for EV and ESS batteries. In UL testing in March 2026, it achieved UL94 V-0 and CTI PLC 0.

CD-110 layer structure: non-combustible surface, heat-resistant fiber and flame-retardant adhesive layers
CD-110 layer structure: non-combustible surface, heat-resistant fiber and flame-retardant adhesive layers. Image: DONGBANG MATERIAL

In May 2026 we launched CD-110, a flexible non-combustible sheet for EV and ESS batteries.

About CD-110

CD-110 is a flexible, non-combustible sheet based on inorganic materials. We developed it as a replacement for mica sheets, which are widely used for fire protection in battery modules and packs.

Mica sheets are made by pressing layers together, which makes them hard to fit to curved surfaces. CD-110 bends, so it can follow the varied shapes inside modules and packs. With an adhesive layer added, it can also be bonded to materials such as PCM and SMC.

UL test results

In UL testing in March 2026, CD-110 achieved the following results.

TestResult
UL94 flammabilityV-0
CTI (tracking resistance)PLC 0
GWIT (glow-wire ignition temperature)850°C
GWFI (glow-wire flammability index)960°C

We developed CD-110 to deliver flame retardancy and electrical insulation in a single material, and these tests confirmed both.

Samples and documents

To request CD-110 samples or test documents, email cs@dbmaterial.com. Include the application, size and quantity you need, and our team will review your request and get back to you.

CD-110 UL test results and bonded structure
CD-110 UL test results and bonded structure. Image: DONGBANG MATERIAL

Press Coverage

Back to list

Quotes and Samples

Tell us the product, grade, quantity and application, and our team will review your request and get back to you.

Email cs@dbmaterial.comFax +82-2-6280-1988